As tiles are getting larger in size nowadays, interior ceramic tiles are often partly broken near joints and regularly cracked on the surface - Tile Side Breakage - after the attachment. In this study, large bathroom in real size was built to measure bond strength and ratio of length change, observe cracks and breakages with naked eye, and conduct the freeze-thaw experiment. Then, these factors were analyzed to identify the cause of Side Breakage and suggest the preventive measure. As a result, cement mortar enhances bond strength of the tile and resistance to cracks, and the more edges which is open, the more cracks tiles develop. Also, the installation of silicon expansion joints is considered as the most effective prevention method of Side Breakage.
목차
Abstract 1. 서 론 2. 실험계획 및 방법 2.1 실험계획 2.2 사용재료 2.3 실험방법 3. 실험결과 및 고찰 3.1 시험체의 길이변화율 3.2 타일 접착강도 3.3 타일 파손의 육안관찰 3.4 동결융해 4. 결 론 참고문헌
대한건축학회지회연합회 [The Regional Association of Architectural Institute of Korea]
설립연도
2000
분야
공학>건축공학
소개
본회는 건축에 관한 학술․ 예술․ 기술을 연구 연마하는 지회회원들의 입지향상과 회원상호간의 친목도모와 함께 건축 문화창달에 기여함을 목적으로 한다.
목적을 달성하기 위하여 다음의 사업을 한다.
1. 지회회원의 입지향상과 친목도모
2. 건축에 관한 조사․연구지도 및 이에 관련된 사업
3. 회지, 논문집, 연구보고서 기타 건축에 관한 도서의 간행
4. 건축에 관한 강습회․강연회․간담회․전람회․견학회 등의 개최
5. 건축에 관한 계획, 감독, 기술검토에 대한 국가공공기관 기타의뢰에 관한 사항
6. 국내외 관계 제 학회와의 교류 및 회의참석
7. 기타 본회 목적달성에 필요한 사업
간행물
간행물명
대한건축학회연합논문집 [Journal of the Regional Association of Architectural Institute of Korea]