The molten marks of electrical wiring found at the fire site can be helpful in inferring the cause of the fire and the ignition point, and it is a very important piece of evidence. However, in the fire department, there are few cases of quantitative analysis and study on the texture of molten marks. In this study, based on the ASTM E1382 standard, using an analysis program called iSolution DT, the image taken with an electron microscope is analyzed and quantitatively determined. In a energized state, the electric wiring was short-circuited at 25°C and 600°C to form molten marks. The primary melt scar shorted at 25°C showed a small columnar structure major axis ratio (GAR), and the secondary melt scar shorted at 600°C showed a large major axis ratio (GAR). As a result, it will be very helpful in quantitatively classifying primary and secondary melt traces using isolution DT.
목차
Abstract 1. 서론 2. 실험 개요 및 실험 방법 2.1 실험 개요 2.2 실험 방법 2.3 실험 결과 및 분석 3. 실험 결과 및 고찰 3.1 구리의 단면 조직 분석 이론 3.2 전선 용융흔(단락흔)의 단면 조직 분석 4. 연구 결과 및 고찰 5. 결론 참고문헌
화재의 과학적 감식, 원인규명 및 예방을 위한 학문과 기술의 발전을 도모하고, 산, 학, 연, 정의 상호 교류를 통한 화재예방과 조사 및 감식의 전문화와 함께 소방관련 정책방향 발전에 공한하며, 회원 및 화재 관련 분야의 국.내외 인사들과의 정보 교류를 위하여 설립되었다.
간행물
간행물명
한국화재감식학회 학회지 [Magazine of Fire Investigation Socity of Korea]