In this study, we investigated the degradation characteristics of KIV, HIV, and HFIX cables according to the temperature and humidity by using accelerated temperature humidity testing method. In order to identify the degradation properties, cables were put into the oven with two different conditions, only temperature stress at 130oC, and temperature-humidity stress at 90oC with 45% RH. the changes in weight, thickness, char length and insulation resistance were measured. Although HFIX cables had weakness of moisture, the insignificant change in weight, length and insulation resistance were measured in the samples under the temperature-humidity stress condition. Therefore, extra experiments including the effects of external condition should proceed in the next research.
목차
Abstract 1. 서론 1.1 연구의 배경 및 필요성 1.2 이론적 배경 1.3 선행연구 1.4 연구의 방법 및 범위 2. 본론 2.1 전기배선의 절연열화 특성확인을 위한 실험 방법 2.2 실험 결과 3. 결론 참고문헌
화재의 과학적 감식, 원인규명 및 예방을 위한 학문과 기술의 발전을 도모하고, 산, 학, 연, 정의 상호 교류를 통한 화재예방과 조사 및 감식의 전문화와 함께 소방관련 정책방향 발전에 공한하며, 회원 및 화재 관련 분야의 국.내외 인사들과의 정보 교류를 위하여 설립되었다.
간행물
간행물명
한국화재감식학회 학회지 [Magazine of Fire Investigation Socity of Korea]