금속의 두께가 도재의 파절강도에 미치는 영향
A study on the differance of Ceramic fracture strength according to the metal depth

첫 페이지 보기
  • 발행기관
    대한치과기공학회 바로가기
  • 간행물
    대한치과기공학회지 바로가기
  • 통권
    Vol.27 No.1 (2005.07)바로가기
  • 페이지
    pp.89-95
  • 저자
    신무학, 최운재, 김용원
  • 언어
    한국어(KOR)
  • URL
    https://www.earticle.net/Article/A60343

※ 기관로그인 시 무료 이용이 가능합니다.

4,000원

원문정보

초록

영어
In the manufacture of ceramo-metal crown, difference of fracture strength according to the metal
depth has been known to be an important influence on enough intensity and internal stress to
endure an occlusion-pressure as well as aesthetics of rehabilitating similar colour such as natural teeth. Depth of ceramic material could be determined by that of metal in three groups: first case of thin depth, second case of thick depth, and third case of constant depth. For the enhancement of the fracture strength between metal and ceramic materials and aesthetic satisfaction, a study on the bonding force, fracture strength, and aesthetics have been required more.
In this study, therefore metal coping were made in three groups of A, B and C by using both
ceramic powder of Norithe and metal of Columbium, which have been used primarily in the
market. A group was made in 0.2 10 10 , B group was made in 0.4 10 10 , and, C group was made in 0.8 10 10 , respectively. The number of metal coping in each group was 10, and total sample numbers used in this study were 30 metal copings. After thesemetal coping tissue were in the process of build-up in 1.5mm constant depth of porcelain, firing, and glazing, the fracture strength about each metal coping tissue was investigated using oil press. It was found that the average values of durable occlusion pressure for separation of ceramic material in the porcelain fused to metal crown (PFM) in the each group showed the increasing order of A group (30 bar), B group (42 bar), and C group (44 bar), respectively. Proper depth of metal coping in the PFM was considered to be 0.4 in the B group because this metal size showed higher durable property to the occlusion pressure and better coupling strength in the ceramo-metal crown.

목차

Abstract
 Ⅰ. 서론
 Ⅱ. 실험재료 및 방법
  1. 실험재료
  2. 실험 방법
 Ⅲ. 실험결과 및 고찰
 Ⅳ. 결론
 참고문헌

키워드

ceramo-metal crown binding stenght according.

저자

  • 신무학 [ Mu-Hak Shin | 원광보건대학 치기공과 ]
  • 최운재 [ Un-Jae Choi | 원광보건대학 치기공과 ]
  • 김용원 [ Yoong-Won Kim | 보화치과기공소 ]

참고문헌

자료제공 : 네이버학술정보

간행물 정보

발행기관

  • 발행기관명
    대한치과기공학회 [The Korean Academy Of Dental Technology]
  • 설립연도
    1979
  • 분야
    의약학>치의학
  • 소개
    본 학회는 치과기공에 관한 모든 분야의 연구와 회무를 총괄하기 위하여 세분화된 분과학회의 회원 상호간 학술교류와 정보를 수집하고, 보수교육 및 학술대회 준비, 진행과 학회지 발간등의 업무를 효율적으로 수행함을 목적으로 한다.

간행물

  • 간행물명
    대한치과기공학회지 [THE JOURNAL OF KOREAN ACADEMY OF DENTAL TECHNOLOGY]
  • 간기
    계간
  • pISSN
    1229-3954
  • eISSN
    2288-5218
  • 수록기간
    1979~2026
  • 등재여부
    KCI 등재
  • 십진분류
    KDC 515 DDC 617

이 권호 내 다른 논문 / 대한치과기공학회지 Vol.27 No.1

    피인용수 : 0(자료제공 : 네이버학술정보)

    함께 이용한 논문 이 논문을 다운로드한 분들이 이용한 다른 논문입니다.

      페이지 저장