자성 연마 마감을 통한 표면 품질 Inconel 625 솔레노이드 밸브 STEM 고속 생산
High-speed Production of Surface Quality Inconel 625 Solenoid Valve STEM via Magnetic Abrasive Finishing
※ 기관로그인 시 무료 이용이 가능합니다.
※ 학술발표대회집, 워크숍 자료집 중 4페이지 이내 논문은 '요약'만 제공되는 경우가 있으니, 구매 전에 간행물명, 페이지 수 확인 부탁 드립니다.
3,000원
원문정보
초록
영어
This research investigates into using a highly efficient magnetic abrasive finishing (MAF) method to refine the surface of an Inconel 625 bar intended for use as a stem in a hydrogen solenoid valve. In contrast to the previous choice of STS 316 material, Inconel 625 was selected due to its superior properties. The cylindrical surface of Inconel 625 bars underwent polishing using the super-fast MAF process, employing varying rotational speeds ranging from 1000 to 25,000 RPM and a potent magnetic field of 550 mT. The study evaluated the polishing outcomes concerning abrasive type, rotational speeds, and processing duration. The results demonstrated the achievement of an exceptionally smooth surface on the Inconel 625 bar, with the surface roughness (Ra) reduced significantly, reaching 0.03 μm under optimal conditions. These conditions included employing carbon nanotube (CNT) particles of 0.04g, PCD diamond abrasive of 1g, Fe of 9g, 0.5g of light oil, and a processing time of 16 minutes at 15,000 RPM. Furthermore, Ansys analysis confirmed the mechanical integrity of the polished Inconel 625 bar, exhibiting suitable strain, equivalent stress, and safety factors. This substantiates the feasibility of employing Inconel 625 bars in hydrogen tanks, surpassing the conventional STS 316L bars.