This study was conducted for the purpose of suggesting a standard that can be used under ambient temperature by improving the low mechanical and thermal properties of ABS. PC was used as a filler, and post-curing conditions of the ABS/PC blend injection material were investigated. It was found that the ABS/PC blend injection material having a PC content of 20 wt.% or more showed little change in tensile properties at a temperature of 50°C, and a decrease in tensile properties of less than 10% at 80°C.