Purpose: The purpose of this study was to evaluate the internal fitness of the resin coping that was fabricated by the traditional and Digital manufacturing methods through 3-dimensional analysis. Methods: maxillary right second molar was chosen implant master model. Custom-built impression trays were manufactured. After screwing the pick-up impression coping onto the master cast, impressions were made with silicone impression. The Working model was then made with type IV stone. The coping was fabricated: SLAC group (n=8), APPC group (n=8), LAPC group (n=8) Resin coping data was measured by using a three-dimensional evaluation program. Internal fitness was calculated by RMS (Root Mean Square).It measures mean and Standard Deviation (SD). Results: Three groups are measured 47.11±(3.08)㎛ total RMS of SLAC group, 48.35(±1.55㎛) for total RMS of LAPC group, 43.45±2.09㎛ for total RMS of APPC group. Measured value is gradually increased. Followed by autopolymerized pattern resin; Stereolithography resin, Light-activated pattern resin But there were no differences stastically(P>0.321). Conclusion: Evaluation of internal fitness on Resin copings was fabricated by three–ways methods showed that no differences statistically significant and clinically acceptable results
목차
[Abstract] Ⅰ. 서론 Ⅱ. 연구 방법 1. 주작업모형의 선정 2. 레진 코핑 시편 제작 3. 디지털3차원 모형 데이터의 제작 4. 3차원적 분석 5. 통계분석 Ⅲ. 결과 Ⅳ. 고찰 Ⅴ. 결론 REFERENCES