Sulfate attack is one of deterioration factors damaged to the concrete durability, especially magnesium sulfate corrosion has known that it arises more serious durability decline by generating de-solidation M-S-H gel. For the purpose of increasing resistance of the sulfate attack, pozzolan has been used, however, there is lake of study on the sulfate resistance of waste glass concrete contained waste glass powder. In this paper, the deterioration degree with digestion's days of waste glass concrete digested in magnesium sulfate solution is observed and analyzed, then compared to plain concrete and concrete contained fly ash and blast furnace slag powder.
목차
Abstract 1. 서론 2. 실험계획 및 방법 2.1 실험계획 2.2 사용재료 2.3 실험방법 3. 실험결과 및 고찰 3.1 콘크리트의 물리적 특성 3.2 황산마그네슘 침식 저항성 4. 결론 참고문헌