As tiles are getting larger in size nowadays, interior ceramic tiles are often partly broken near joints and regularly cracked on the surface - Tile Side Breakage - after the attachment. In this study, large bathroom in real size was built to measure bond strength and ratio of length change, observe cracks and breakages with naked eye, and conduct the freeze-thaw experiment. Then, these factors were analyzed to identify the cause of Side Breakage and suggest the preventive measure. As a result, cement mortar enhances bond strength of the tile and resistance to cracks, and the more edges which is open, the more cracks tiles develop. Also, the installation of silicon expansion joints is considered as the most effective prevention method of Side Breakage.
목차
Abstract 1. 서 론 2. 실험계획 및 방법 2.1 실험계획 2.2 사용재료 2.3 실험방법 3. 실험결과 및 고찰 3.1 시험체의 길이변화율 3.2 타일 접착강도 3.3 타일 파손의 육안관찰 3.4 동결융해 4. 결 론 참고문헌
저자
신상엽 [ Shin, Sang-Yeop | 정회원, 부산대학교 건축공학과 석사과정 ]
정의창 [ Jung, Euy-Chang | 정회원, 부산대학교 건축공학과 석사과정 ]
김영수 [ Kim, Young-Su | 정회원, 부산대학교 건축학부 교수, 공학박사 ]
교신저자